Corrosion-resitant, Shiny, Toxic | 100 sec. gravel, 140 sec. arsenic | (tested on Copper) |
Ductile, Non-toxic | 270 sec. lime | (tested on Tin) |
Ductile, Non-toxic | 190 sec. lime | (tested on Copper) |
Ductile, Shiny, Stainless | 165 sec. Gravel, 25 sec. lime, 20 sec. Arsenic | (tested on Strontium) |
Ductile, Plastic | 100 sec. Gravel, 25 sec. lime, 75 sec. Cabbage juice, 7 sec. lime | (tested on Zinc) |
Hard Corrosion Resistant Insulative Nontoxic | 130 sec. Sap, 10 sec. gravel | ( Tested on Tungsten) |
Hard Nontoxic | 270 sec. Catcus Sap | (tested on Lead) |
Hard Stainless Nontoxic | 140 sec. Cactus Sap, 30 sec. Arsenic | (tested on Copper) |
Shiny Corrosion-resistant Insulative | 150 sec. gravel | ( Tested on Strontium) |
Stainless Plastic | 150 sec. gravel, 150 sec. potash, 70 sec. salt | ( Tested on Copper) |
Corrosion-resistant Insulative | 45 sec. gravel | ( Tested on Antomony) |
Shiny Corrosion-resistant Insulative | 200 sec. gravel | ( Tested on Iron) |
Shiny Plastic Insulative | 160 sec. gravel, 55 sec. cabbage juice | ( Tested on Aluminium) |