Add recipes for Metal Treatment here

Listed in seconds (not amounts) and need to be inputed in this order

Shiny Conductive Purity 6 Platinum Plated Moonsteel

Tank 2:

This will yield 60% Metal Blue.

Moonsteel with at least 13 seconds of salts of platinum already in the acid.

Aluminum Plated, Stainless, Toxic, Hard, Purity 6. Metal Blue

Tank 2:

With at least 13 seconds of salts of Aluminum already in the tank.

Tungsten Plated, Stainless, Tarnished, Hard, Purity 6. Metal Blue

Tank 2:

With at least 4 seconds of salts of Tungsten already in the tank.

Plastic, Conductive, Silver-plated, Purity 10, Titanium

Tank 1:

This will all become Water Metal.

Insulative, Stainless, Sun Steel

Tank 1:

Ductile, Hard, Stainless, Thoth's Metal

Tank 1:

Hard, Corrosion Resistant, Pewter

Tank 1:

Hard, Nontoxic, Moonsteel

Tank 1:


Home | Atlas | Guides | Tests | Research | Techs | Skills | Index | Recent Changes | Preferences | Login
You must log in to edit pages. | View other revisions
Last edited October 20, 2008 9:30 pm by EldradUlthran (diff)
Search: